Trouble Shooting of Coating Failures

   
 
Problem Cause Solution
Coating peels. Coating is too thick. Dilute coating mixture so that the layer thickness does not exceed 100µm.
Coating does not adhere on the surface. Bad surface conditions. Clean and degrease surface,   heat surface prior to application to 100-150°C.
Further layers do not stick on the first layer. First coating is not  completely dried. Extend drying time, remove loose particles and coat again.
Coating cracking. Coating mixture is too thick. Dilute coating mixture in such way that thinner layers can be applied.
Cloudy, uneven application when spraying. Coating mixture is not stirred up, spray gun is led jerkily not uniform. Stir coating mixture or use a mixer. Pull even courses with spray gun.
   
 
 
 
  PRODUCTS
   
BORON OXIDE GLASS
TURBOSTRATIC BORON NITRIDE
HEXAGONAL BORON NITRIDE
BORTEK 11
BORTEK 01
BORTEK W01
BORONMAX
   
Copyright © BORTEK BORON TECHNOLOGIES and MECHATRONICS INC. - www.borteknolojileri.com